Brass
Brass Low Brass, 80%
Buy MetalAnnealing Procedure
The annealing temperature for this alloy is between 800 and 1300 F.
Cold Workability
The capacity for cold working this alloy is rated as "excellent".
Forgeability
The hot forgeability rating of this alloy is unknown. (Forging Brass=100). The recommended hot working temperature for this alloy is between 1500 and 1650 F.
Hot Workability
This alloy's capacity for being hot formed is rated as "fair".
Machinability
The machinability rating of this alloy is 30. (Where Alloy 360 FC Brass is 100).
Principle Design Features
Brasses (Copper-Zinc Alloy), Low Brass, 80%. Similar to, but stronger than C23000.
Weldability
Soldering is rated as "excellent", brazing is rated as "excellent", oxyacetylene welding is rated as "good", gas shielded arc welding is rated as "good", coated metal arc welding is "not recommended", spot welding is rated as "fair", seam welding is "not recommended" and butt welding is rated as "good".
Known Forms
Coil
Disc
Flat Bar
Foil
Hexagon Bar
Hollow Bar
Pipe
Plate
Ring
Rod
Round Bar
Round Tube
Sheet
Square Bar
Strip
Additional Data
Specifications
B134,B36,W321,J461,J463,C24000Chemical Elements
| Copper | 78.5 - 81.5 |
| Iron | 0.05 max |
| Lead | 0.05 max |
| Remainder Each | Zn |
Physical Properties
Density: 0.313lb/in³
Electrical Resistivity: 32.5µΩ·cm
Melting Point: 1770°F
Mechanical Properties
Modulus of Elasticity – Tension: 16MSI