Bronze
Bronze C70600
Annealing Procedure
The annealing temperature for this alloy is between 1100 and 1500 F.
Applications
Copper-nickels are mainly used for seawater service as forged and machined valve and pump components, fittings and hardware. Used where high corrosion resistance is required and where concern over chloride stress-corrosion cracking prevents use of stainless steels.
Cold Workability
The capacity for cold working this alloy is rated as "good".
Forgeability
The hot forgeability rating of this alloy is unknown. (Forging Brass=100). The recommended hot working temperature for this alloy is between 1550 and 1750 F.
Hot Workability
This alloy's capacity for being hot formed is rated as "good".
Machinability
The machinability rating of this alloy is 20. (Where Alloy 360 FC Brass is 100).
Principle Design Features
Copper Nickels (Copper-Nickel), Copper-Nickel, (90-10). Excellent corrosion resistance, especially in marine environments. Moderately high strength, good creep resistance at elevated temperatures. Properties generally increase with nickel content. Relatively high in cost compared with copper-aluminum and other alloys with similar mechanical properties.
Weldability
Soldering of this alloy is rated as "excellent", brazing is rated as "excellent", oxyacetylene welding is rated as "fair", gas shielded arc welding is rated as "excellent", coated metal arc welding is rated as "good", spot welding is rated as "good", seam welding is rated as "good", and butt welding is rated as "excellent".
Known Forms
Coil
Disc
Flat Bar
Foil
Hexagon Bar
Hollow Bar
Pipe
Plate
Ring
Rod
Round Bar
Round Tube
Sheet
Square Bar
Strip
Additional Data
Specifications
SB111,SB171,SB359,SB395,SB466,SB467,SB543,B111,B122,B151,B171,B359,B395,B432,B466,B469,B543,B608,2.0872,C-15726,T-15005,T-16420,T-22214,J461,J463,C70600Chemical Elements
| Iron | 1 - 1.8 |
| Lead | 0.05 max |
| Manganese | 1 max |
| Nickel | Includes Co |
| Remainder Each | Cu, including Ag |
| Remainder Total | Cu + sum of named elements 99.5 min |
| Zinc | 1 max |
Physical Properties
Density: 0.323lb/in³
Electrical Resistivity: 112.9µΩ·cm
Mechanical Properties
Modulus of Elasticity – Tension: 18MSI