Nickel Alloy 42 (Ni-Fe Alloy)
Buy MetalAnnealing Procedure
Anneal at 1450F (788C) followed by air cooling.
Applications
Used for glass-to-metal sealing of components that are enclosed in a glass envelope, such as lamps and electron tubes.
Cold Workability
The alloy has good ductility and is readily cold worked.
Forgeability
Forging may be done at 2200 F. As is true of all the high nickel content alloys care should be taken to avoid contamination from sulfur due to long soaking time in a furnace atmosphere.
Formability
Ductility and thus formability are very good.
Hardening Procedure
Hardens due to cold working only.
Heat Treatability
An annealing heat treatment may be used. The alloy is not hardenable by heat treatment.
Machinability
The alloy is readily machinable by conventional techniques.
Principle Design Features
This is an iron-nickel alloy with controlled thermal expansion properties.
Weldability
The alloy may be welded by conventional methods.
Known Forms
Coil
Disc
Flat Bar
Foil
Hollow Bar
Pipe
Plate
Rectangle Tube
Ring
Rod
Round Bar
Round Tube
Sheet
Square Bar
Strip
Additional Data
Specifications
B388,F30,K94100Chemical Elements
| Carbon | 0.05 max |
| Iron | Balance |
| Manganese | 1 max |
| Nickel | 41 nom |
| Silicon | 0.2 nom |
Physical Properties
Density: 0.293lb/in³
Electrical Resistivity: 494µΩ·cm
Melting Point: 2600°F
Specific Gravity: 8.12
Specific Heat: 0.12BTU/lb·°F
Mechanical Properties
Modulus of Elasticity – Tension: 21.5MSI
Thermal Expansion: 0.8µin/in·°F
Thermal Conductivity
| Condition | Temperature | Conductivity |
|---|---|---|
| Annealed | 70 °F | 7.45 BTU/hr·ft·°F |
Thermal Expansion
| Condition | Min | Max | Expansion Coefficient |
|---|---|---|---|
| Annealed | 70 °F | 212 °F | 2.9 μin/in·°F |
| Annealed | 70 °F | 650 °F | 3 μin/in·°F |